AUROKARAT 18 E, bright acid thick gold plating process creates a homogeneous covering, excellent shine and non-tarnishing coatings in 22.5 carat gold color. It is widely used in the electrical, electronics and jewelry industries, especially due to the high friction resistance of the products coated with this process. A preliminary gold bath is recommended to ensure that this bath does not get dirty and has a long life. Some features of the coating are as stated in the table.
| PURITY, HARDNESS | 93.75, 230 - 250 (mHV20) | SPECIFIC GRAVITY | 17.2 gr/cm³ |
| ALLOYING METAL | cobalt | PLATING RATE | 20 mg/Amperminute |
| ANODE CURRENT DENSITY | 0.25 A/dm² | 1 Mikron , 1 A/ dm² | 8.5 minutes |
| PLATING FOR 1 MICRON | 172 mg/dm² gold Consumption | COLOR | RICH YELLOW |